For increasing temperatures due to downsizing, materials are pushed beyond their limits. PVD coatings help to extend the limits even further by reducing wear.
Choose your country / language
For increasing temperatures due to downsizing, materials are pushed beyond their limits. PVD coatings help to extend the limits even further by reducing wear.
Skiktalternativ | Beläggningsmaterial | Beläggningsteknik | Beläggningshårdhet HIT [GPa] | Friktionskoefficient (torr) vs. stål | Max. driftstemp. [°C] | Processtemperatur [°C] | |
---|---|---|---|---|---|---|---|
MoN | Sputter / Arc | 15 – 35 beroende på applikation | - | 800 | - | ||
CrN / a-C:H | PACVD | ~15-25 | 0.1 - 0.2 | 300 | < 250 |