Solution | Coating material | Coating technology | Coating hardness HIT [GPa] | Coefficient of friction (dry) vs. steel | Max. service temp. [°C] | Process temperature [°C] | |
---|---|---|---|---|---|---|---|
MoN | Sputter / Arc | 15 – 35 depending on application | - | 800 | - | ||
CrN / a-C:H | PACVD | ~15-25 | 0.1 - 0.2 | 300 | < 250 |