BALINIT and BALIFOR coatings allow modifications in the system design. This results in less components needing to be assembled.
Choose your country / language
BALINIT and BALIFOR coatings allow modifications in the system design. This results in less components needing to be assembled.
Soluzione | Materiale di rivestimento | Tecnologia Coating | Durezza rivestimento HIT [GPa] | Coefficiente di attrito (asciutto) rispetto all'acciaio | Temp. max. di servizio [°C] | Temperature di processo [°C] | |
---|---|---|---|---|---|---|---|
CrN / a-C:H | PACVD | ~15-25 | 0.1 - 0.2 | 300 | < 250 | ||
ta-C | Arc | > 40 | 0.1 - 0.2 | 450 | - | ||
MoN | Sputter / Arc | 15 – 35 depending on application | - | 800 | - |