\uf1ad
Please select your suitable product
×
×
Solution Coating material Coating technology Microhardness HIT (GPa) Coefficient of friction (dry) vs. steel Max. service temp. [°C] Process temperature
BALIMED A TiN Arc 30 +/- 3 ~ 0.6 600 < 350
BALIMED DLC a-C:H PACVD ~ 15 - 25 0.1 - 0.2 300 < 250
BALIMED C a-C:H:W (WC/C) Sputter 8-12 / 12-15 0.1 - 0.2 300 < 250
BALIMED FUTURA TiAlN Arc 33 +/- 3 0.6 700 < 350
BALIMED ARGENTA TiN:Ag Arc 25 - 29 ~ 0.5 - < 350
BALIMED TICANA TiCN S3p ≥ 35 ~ 0.6 - < 400
image

Dental instruments and tools

Improved life time of instruments

  • High wear and abrasion resistance
  • Better identification through colour coding
  • Chemically stable coatings

Download our BALIMED brochure