Solution Coating material Coating technology Coating hardness HIT [GPa] Coefficient of friction (dry) vs. steel Max. service temp. [°C] Process temperature [°C]
C-based (sp3) CVD 80 - 100 - 600 < 900
Download
C-based (sp3) CVD 80 - 100 - 600 < 900
Download
C-based (sp3) CVD 80 - 100 - 600 < 900
Download
TiN Arc 30 +/- 3 ~0.6 600 < 500
- - - - - -
Download
AlCrN-based Arc 44 +/-4 - 1100 < 500
Download
- - - - - -
Download
TiCN Arc 37 +/-3 - 400 < 500
a-C:H:Me (WC/C) Sputter 10 - 15 0.1 - 0.2 300 < 250
Download
CrN Arc 25+/-3 ~0.5 700 500
Download
CrN Sputter 18+/-3 ~0.5 700 < 250
CrN Arc 18+/-3 ~0.5 700 -
AlCrN Arc - 0.35 1100 -
Download
AlTiN / TiSiXN Arc 37 ± 3 - 1000 -
Download
a-C:H:Si PACVD ~ 15-25 0.05 - 0.2 350 < 220
Download
CrAlN-based Arc 28 +/-2 0,35 900+ -
Download
TiAlN Arc 33 +/- 3 ~0.6 900 500
ta-C Arc 50 - 60 0.1 - 0.2 500 < 150
Download
AlTiN-based Arc 35 +/-3 - 1000 < 500
Download
TiAlN Arc 33 +/- 3 - 900 -
Download
ta-C Arc > 65 < 0.10 > 500 < 150
Download
CrN/CrON Arc 28 +/-3 ~0.5 700 350
Download
AlTiN-based Arc 35 +/-3 - 1000 < 600
Download
AlTiN / TiSiXN Arc 38 +/-5 - 1100 < 600
Download
a-C:H PACVD ~15-25 0.1 - 0.2 300 < 250
CrN / a-C:H PACVD ~15-25 0.1 - 0.2 300 < 250
Download
AlCrN-based S3p 37 +/-3 - 1100 < 500
Download
AlTiN-based S3p 36 +/-3 - 1000 < 500
Download
AlCrN + WC/C S3p 35 +/-2 / 18 +/-1 - 1100 (AlCrN) < 500
Download
AlCrTiN-based S3p 30 +/- 3 - 600 < 500
Download
CrN S3p - 21 +/- 3 0.5 700 -
TiN S3p - 30 +/- 3 0.6 700 -
AlTiSiN-based S3p 38 +/-1 - 1000 < 500
Download
- - - - - -
Download
- - - - - -
Download