| Solution | Coating material | Coating technology | Coating hardness HIT [GPa] | Coefficient of friction (dry) vs. steel | Max. service temp. [°C] | Process temperature [°C] | |
|---|---|---|---|---|---|---|---|
| C-based (sp3) | CVD | 80 - 100 | - | 600 | < 900 | ||
| C-based (sp3) | CVD | 80 - 100 | - | 600 | < 900 | ||
| C-based (sp3) | CVD | 80 - 100 | - | 600 | < 900 | ||
| TiN | Arc | 30 +/- 3 | ~0.6 | 600 | < 500 |
|
|
| AlCrN-based | Arc | 44 +/-4 | - | 1100 | < 500 | ||
| TiCN | Arc | 37 +/-3 | - | 400 | < 500 |
|
|
| AlTiN / TiSiXN | Arc | 37 ± 3 | - | 1000 | - | ||
| AlTiN-based | Arc | 35 +/-3 | - | 1000 | < 500 | ||
| ta-C | Arc | > 65 | < 0.10 | > 500 | < 150 | ||
| TiAlN-based | Arc | 42 +/-2 | - | 1100 | < 500 | ||
| AlTiN / TiSiXN | Arc | 38 +/-5 | - | 1100 | < 600 | ||
| AlCrN-based | S3p | 37 +/-3 | - | 1100 | < 500 | ||
| AlTiN-based | S3p | 36 +/-3 | - | 1000 | < 500 | ||
| AlCrN + WC/C | S3p | 35 +/-2 / 18 +/-1 | - | 1100 (AlCrN) | < 500 | ||
| AlCrTiN-based | S3p | 30 +/- 3 | - | 600 | < 500 | ||
| AlTiSiN-based | S3p | 38 +/-1 | - | 1000 | < 500 |