Solution Coating material Coating technology Coating hardness HIT [GPa] Coefficient of friction (dry) vs. steel Max. service temp. [°C] Process temperature [°C]
- - - - - -
Download
AlCrN-based Arc 44 +/-4 - 1100 < 500
Download
- - - - - -
Download
TiCN Arc 37 +/-3 - 400 < 500
CrN Arc 25+/-3 ~0.5 700 500
Download
CrN Arc 18+/-3 ~0.5 700 -
AlCrN Arc - 0.35 1100 -
Download
CrAlN-based Arc 28 +/-2 0,35 900+ -
Download
TiAlN Arc 33 +/- 3 ~0.6 900 500
TiAlN Arc 33 +/- 3 - 900 -
Download
ta-C Arc > 65 < 0.10 > 500 < 150
Download
CrN / a-C:H PACVD ~15-25 0.1 - 0.2 300 < 250
Download
AlCrN-based S3p 37 +/-3 - 1100 < 500
Download
- - - - - -
Download
- - - - - -
Download