\uf1ad
Please select your suitable product
×
×
×
×
Solution Coating material Coating technology Microhardness HIT (GPa) Coefficient of friction (dry) vs. steel Max. service temp. [°C] Process temperature
BALINIT DLC STAR CrN / a-C:H PACVD ~15-25 0.1 - 0.2 300 < 250
BALIFOR T ta-C Arc > 40 0.1 - 0.2 450 -
BALIFOR M MoN Sputter / Arc 15 – 35 depending on application - 800 -
image

Piston Pins