Choose your country / language

BALINIT FUTURA NANO

The high hardness and tenacity of BALINIT® FUTURA NANO gives outstanding protection against abrasive wear and erosion, making it ideal for highly stressed precision components even under high thermal conditions.  This is also the major benefit for plastic injection moulding and HSS and carbide tools.

The titanium aluminium nitride (TiAlN) structure results in an optimal relation of high hardness to residual compressive stress. This gives great performance especially for highly stressed components and metal forming tools.

For temperature-sensitive components BALINIT® FUTURA NANO ARCTIC is available with a coating temperature of only 200 °C.

BALINIT FUTURA NANO
Material de recubrimiento TiAlN
Tecnología de recubrimiento Arc
Color del recubrimiento violet-grey
Dureza recubrimiento HIT [GPa]* 33 +/- 3
Coeficiente de fricción (en seco) frente al acero** ~0.6
Temp. máx. de trabajo [°C]**** 900
Temperatura de proceso [°C] 500
Observaciones generales Todos los datos aportados son valores aproximados, dependen de la aplicación, el entorno y las condiciones de prueba.
*Dureza recubrimiento HIT [GPa] Medido mediante nano indentación de acuerdo con la norma ISO 14577. Para multicapas, la dureza de las diferentes capas varía.
**Coeficiente de fricción (en seco) frente al acero Determinado mediante “pin on disc” en seco con una bola de acero de acuerdo con ASTM G99. En uso prolongado los valores dados pueden superarse.
****Temp. máx. de trabajo [°C] Estos son valores aproximados en condiciones de laboratorio. Debido a las leyes de la termodinámica existe una dependencia de la presión en la aplicación.

¿Comentarios o preguntas? ¡Contacte con nosotros!

keyboard_arrow_up