\uf1ad

BALINIT CROMA / CROMA PLUSWith BALINIT CROMA, your plastics processing will be in top form even for large components.

×

Whether injection moulding, extrusion or blow moulding - only top quality surfaces ensure optimal manufacturing productivity and efficiency. BALINIT® CROMA and BALINIT® CROMA PLUS are thus the best choices for successful plastics processing, even for large components.

CROMA and CROMA PLUS reduce tool, production and maintenance costs, making them the ideal coatings for PVC window frame and plastic extrusion, and for rubber processing.

  • Advantages

    Advantages

    Extreme coating hardness

     

    High-level protection from abrasive wear

    Protection from wear due to cleaning processes and tool damage

    Multi-layer structure

     

    Significantly less corrosion due to a chemically saturated, dense multi-layer structure

    Low coefficient of friction

     

    The molding materials show very good sliding behaviour on the tool surfaces

    First-class surface properties

     

    Excellent adhesion

    Surfaces with low reactivity

    Significant reduction of deposits

  • Specifications

    Specifications

    BALINIT CROMA
    Coating material CrN
    Coating colour silver-grey
    Coating hardness HIT[GPa]* 25+/-3
    Coefficient of friction (dry) vs. steel** ~0.5
    Max. service temp. [°C]**** 700
    General remark All given data are approximate values, they depend on application, environment and test condition.
    *Coating hardness HIT[GPa] Measured by nano indentation according to ISO 14577. For multilayers the hardness of the different layers varies.
    **Coefficient of friction (dry) vs. steel Determined by ball-on-disc test in dry condition with an Steel ball according to ASTM G99. During run-in the given values may be exceeded.
    ****Max. service temp. [°C] These are approximate values out of the field. Due to thermodynamic laws there is a dependency of pressure in application.
    BALINIT CROMA PLUS
    Coating material CrN + OX
    Coating colour rainbow
    Coating hardness HIT[GPa]* 25+/-3
    Coefficient of friction (dry) vs. steel** ~0.5
    Max. service temp. [°C]**** 700
    General remark All given data are approximate values, they depend on application, environment and test condition.
    *Coating hardness HIT[GPa] Measured by nano indentation according to ISO 14577. For multilayers the hardness of the different layers varies.
    **Coefficient of friction (dry) vs. steel Determined by ball-on-disc test in dry condition with an Steel ball according to ASTM G99. During run-in the given values may be exceeded.
    ****Max. service temp. [°C] These are approximate values out of the field. Due to thermodynamic laws there is a dependency of pressure in application.
  • Downloads
  • Application

    Recommendation Application

    Tools applications

    • Plastics processing Plastics processing

      The benchmark for injection moulding and extrusion

      Details
  • Contact us
    Contact us via phone

    +423 388 7500

    Contact us via mail

    We would be pleased to hear from you. Please enter your personal details.



    Oerlikon Surface Solutions AG
    Pfaeffikon, Branch Balzers
    Iramali 18
    9496 Balzers
    Liechtenstein

Coating Guide