BALINIT X.CELL BALINIT X.CELL expressly addresses the wide-ranging requirements of forming techniques:

BALINIT X.CELL thick sheets and sheets with high tensile strength or surface pre-treatment can be processed with higher stroke rates and longer service life. In dry forming operations the surface quality of the worked pieces is improved.
Coating Properties
Coating Material TiCrN
Microhardness* (HV 0.05) 2,100
Friction coefficient* against steel (dry) 0.30 – 0.35
Max. service temperature (°C) 700
Coating colour dark grey

* depends on application and test conditions

Recommended applications:
  • tools for demanding sheet metal forming